ZWCNC TECHNICAL ARCHIVE

Shearing Burr and Squareness: Symptom-First Diagnostic Record

A safe evidence record for distinguishing full-length burr, one-sided burr, tapered strip width, bow/twist and repeated-length drift. It organises material, blade, hold-down, backgauge and sample measurements before qualified adjustment or service.

Hydraulic guillotine and swing-beam shears2026-08-31ZWCNC symptom-first diagnostic record

What this reference covers

  1. 1Heavy burr distributed along the complete cut
  2. 2Burr or edge deformation concentrated on one side
  3. 3Cut strip width taper from front to rear or left to right
  4. 4Workpiece bow, twist or rollover after shearing
  5. 5Repeated cut-length drift or inconsistent backgauge result

Field verification checklist

Lock out power and release stored energy before entering blade, hold-down or rear danger zones
Record model, serial number, blade type/condition, material grade, batch, thickness, cut length and approved clearance method
Measure burr height and strip width at fixed labelled positions rather than judging one point
Verify hold-down contact, material support, reference-edge contact and backgauge repeatability without bypassing safeguards
Change or adjust blades and clearance only by the machine-specific procedure; escalate cracks, chipped blades, hydraulic leaks or abnormal motion