What this reference covers

  1. 1MFSC and MFMC source families from 1000 to 30000 W
  2. 2Carbon steel, stainless steel, aluminium and brass examples
  3. 3Speed, power, gas, pressure, nozzle, focus and cut height
  4. 4Core-diameter and optical-configuration dependencies
  5. 5Multi-stage piercing references and database cautions

Field verification checklist

Use every table value only as a controlled starting point
Match source, core diameter, collimation, focus, head and nozzle
Confirm real material grade, surface condition and gas purity
Run coupon tests and inspect piercing, dross, kerf and heat effect
Record approved parameters by machine, material batch and quality requirement